104
submitted 2 days ago* (last edited 1 day ago) by dual_sport_dork@lemmy.world to c/justpost@lemmy.world

Let's have a different flavor of insanity around here for a change. Besides, where else am I going to yammer about this? Somehow it feels a bit, uh, insufficiently effortful to put this in either of my usual haunts.

I ground three knives yesterday. In so doing I generated this pile of metal dust and it is deeply strange.

Of course, generating piles of metal dust is standard operating procedure around here these days, but the way this alloy behaves is just so damn weird.

The nasty coarse 24 grit belt I use to do my rough beveling produces little hair-thin spiral filaments of this stuff that simultaneously remind me of steel wool and/or microscopic drilling chips. This is completely different from the usual powder I wind up with. As they pile up they interlock and I discovered this curious property when I went to vacuum the stuff up and it wouldn't vacuum. This entire lump, which is about 8" in diameter and at least 3" thick, was matted into a single metallic Tribble that also completely resisted my attempt to stab a ruler into it to measure its height. Ultimately I was able pick pretty much the entire thing up in one piece after some expenditure of effort in un-Velcroing it from the carpet, and chucked it into the trash whole.

(Yes, that is a disused floor mat from a car I intentionally fire my metal shavings into, nominally so I can slide it out my shop door and thwap it against the side of the building to do away with the normal types of metal dust. It's from a RAV4, if you must know.)

Suddenly and for no particular reason I can put my finger on, I'm feeling very vindicated in my decision these days to wear a respirator while grinding.

you are viewing a single comment's thread
view the rest of the comments
[-] ICastFist@programming.dev 7 points 2 days ago

What uses can that dust have? Best I can think of is mixing with some resin and throwing down a mold

[-] mercano@lemmy.world 4 points 1 day ago

Steel wool works as fire starter because of its very high surface area to volume ratio. I imagine you could do the same with metal dust, at least certain alloys. The space shuttle SRBs were packed with a mix of aluminum dust fuel and ammonium perchlorate oxidizer, along with some epoxy binder & iron oxide catalyst.

[-] dual_sport_dork@lemmy.world 7 points 2 days ago

That would certainly work if you were looking for the grey and gritty vibe. I imagine the fibers are long enough that they actually might serve as real functional reinforcement in the resin as well.

[-] Assassassin@lemmy.dbzer0.com 0 points 2 days ago

If you had the requisite skills, you could just re-cast it?

[-] dual_sport_dork@lemmy.world 6 points 2 days ago

Casting it would require making it bloody hot. An awful lot of it has oxidized as well, because it has a high surface area and the shavings started life as grinder sparks, i.e. being actively on fire while on their way to the floor.

So yes, but you'd wind up with a lot of slag. It might be best to start with an even bigger pile in that case.

[-] Godort@lemmy.ca 6 points 2 days ago

If a sufficient portion of it is oxide, you could mix it with aluminum dust to make a shitty, but serviceable thermite

this post was submitted on 23 Nov 2026
104 points (98.1% liked)

Just Post

1707 readers
412 users here now

Just post something ๐Ÿ’›

Lemmy's general purpose discussion community with no specific topic.

Sitewide lemmy.world rules apply here.

Additionally, this is a no AI content community. We are here for human interaction, not AI slop! Posts or comments flagged as AI generated will be removed.

founded 3 years ago
MODERATORS